The principle of the AAS method consists in inspiration of the test solution into an acetylen/air flame. Measurement of the absorption of the selected spectral line emitted by a cadmium hollow-cathode or cadmium discharge lamp, in the region of 228,8 nm. The principle of the polarographic method consists in electrolysis of the test solution in a polarographic cell measurement of the corresponding heigth of the potential step. The method are applicable to coating materials having "soluble" cadmium contents in the range of about 0,05 % (m/m) to 5 % (m/m). The AAS method should be used as the referee method in cases of dispute. This second edition cancels and replaces ISO 3856/4-1980.


Общая информация

  • Текущий статус :  Published
    Дата публикации : 1984-10
  • Версия : 2
    Число страниц : 6
  • :
    ISO/TC 256
    Pigments, dyestuffs and extenders
  • 87.040
    Paints and varnishes

Приобрести данный стандарт

Формат Язык
PDF
Бумажный
  • CHF38

Жизненны цикл

Стандарт, который пересматривается каждые 5 лет



Изменения / Исправления

Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)

Будьте в курсе актуальных новостей ИСО

Подписывайтесь на наши новости, обзоры, а также на информацию о продуктах